Skip to main content

BAM Creep Test Parser

An openBIS parser for creep testing data in BAM.

A tutorial in tutorials/parser_tutorial.py help parsing the Creep Excel files into the BAM openBIS instance. This tutorial uses the parser class defined in src/creep_test_parser/parser.py and the bam-masterdata parser infrastructure.

Development

If you want to develop locally this package, clone the project and enter in the workspace folder:

git clone https://github.com/BAMresearch/creep-test-parser.git
cd creep-test-parser

Create a virtual environment (you can use Python>=3.10) in your workspace:

  • Using venv:
    python3 -m venv .venv
    source .venv/bin/activate  # in Windows (cmd): source .venv\Scripts\activate
    
  • Using conda:
    conda create --name .venv pip
    conda activate .venv
    

Install the package in editable mode (with the flag -e):

pip install --upgrade pip
pip install -e '.[dev]'

Note: In order to install faster the package, you can use uv for pip installing Python packages:

pip install --upgrade pip
pip install uv
uv pip install -e '.[dev]'

Run the tests

You can locally run the tests by doing:

python -m pytest -sv tests

where the -s and -v options toggle the output verbosity.

You can also generate a local coverage report:

python -m pytest --cov=src tests

Run auto-formatting and linting

We use Ruff for formatting and linting the code following the rules specified in the pyproject.toml. You can run locally:

ruff check .

This will produce an output with the specific issues found. In order to auto-fix them, run:

ruff format .

If some issues are not possible to fix automatically, you will need to visit the file and fix them by hand.

Metadata

Release files for creep-test-parser 1.0.0

For a detailed explanation of source distributions (sdists) and built distributions (wheels), please see the package formats documentation.

Source distribution (sdist)

Source distribution for creep-test-parser 1.0.0
File Size Uploaded Provenance
creep_test_parser-1.0.0.tar.gz 82.2 kB With provenance Details

Built distribution (wheel)

Table of built distributions (wheels) for creep-test-parser 1.0.0
File Interpreter ABI Platform
creep_test_parser-1.0.0-py3-none-any.whl Python 3 none any Details

Total release size: 95.4 kB

Release files / creep_test_parser-1.0.0.tar.gz

Download URL creep_test_parser-1.0.0.tar.gz
Size 82.2 kB
Tags Source
SHA-256 checksum
How to use checksums
728f791ef864ed0a975db2e7c85fef80b40df1e211dc186ddb1c53109ed24904
BLAKE2b-256 checksum
How to use checksums
291ab2b730f997c8be7d907a7b593b818e39b010aae77b086f9186a9ffb6b3ee
Upload date
Uploaded using Trusted Publishing?
What is trusted publishing?
Yes
Uploaded via twine/7.0.0 CPython/3.13.16

Provenance

Provenance describes where a file came from. On PyPI, provenance is shared via attestations, which provide a verifiable record of the build or publishing details. View details, limitations and caveats.

PyPI Publish Attestation

PyPI verified that this artifact, at this checksum, originated from the publisher listed below.

Signed by GitHub Actions, verified by PyPI on Oct 22, 2026.

Transparency log

Release files / creep_test_parser-1.0.0-py3-none-any.whl

Download URL creep_test_parser-1.0.0-py3-none-any.whl
Size 13.2 kB
Tags Python 3
SHA-256 checksum
How to use checksums
997f5827f2915d6a031cbf2bfff35adcbae8dbe803c6956c17c25e94bfcf8955
BLAKE2b-256 checksum
How to use checksums
845dcae03039870056f2d945a47ff1d4238a2ab1789e38547c64c00c93bb1cfb
Upload date
Uploaded using Trusted Publishing?
What is trusted publishing?
Yes
Uploaded via twine/7.0.0 CPython/3.13.16

Provenance

Provenance describes where a file came from. On PyPI, provenance is shared via attestations, which provide a verifiable record of the build or publishing details. View details, limitations and caveats.

PyPI Publish Attestation

PyPI verified that this artifact, at this checksum, originated from the publisher listed below.

Signed by GitHub Actions, verified by PyPI on Oct 22, 2026.

Transparency log

Security for creep-test-parser 1.0.0

Provenance

Provenance describes where a file came from. On PyPI, provenance is shared via attestations, which provide a verifiable record of the build or publishing details. View details, limitations and caveats.

Full provenance

All 2 files in this release have been uploaded with provenance metadata.

Select from 2 files

Attestation for creep_test_parser-1.0.0.tar.gz

PyPI Publish Attestation

PyPI verified that this artifact, at this checksum, originated from the publisher listed below.

Signed by GitHub Actions, verified by PyPI on Oct 22, 2026.

Transparency log

A note on package security

PyPI is a repository for distributing packages, not a service for auditing them. While third-party security researchers and our staff do their best to detect and remove malicious packages, PyPI cannot guarantee the quality, security or suitability of any given package.

Release history Release notifications | RSS feed

This release

1.0.0 This release

2 release files Full provenance

Anthropic, PBC Visionary sponsor Bloomberg Visionary sponsor Hudson River Trading Visionary sponsor Meta Visionary sponsor NVIDIA Visionary sponsor Microsoft Sustainability sponsor Depot Continuous Integration AWS Cloud computing and Security Sponsor Datadog Monitoring Fastly CDN Google Download Analytics Sentry Error logging StatusPage Status page